产品详情
理性指标
| 项目 | 指标 | |||||||
| N-1 | N-2a | N-2b | N-3a | N-3b | N-4 | N-5 | ||
| 耐火度°C≥ | 1750 | 1730 | 1730 | 1710 | 1710 | 1690 | 1670 | |
| 0. 2 MPA荷重软 化开始温度≥ | 1400 | 1350 | 1320 | 1300 | ||||
| 重烧线变化% |
1400°C 2 h |
+0.1 -0.4 |
+0.1 -0.5 |
+0.2 -0.5 |
||||
|
1350°C 2 h |
+0.2 -0.5 |
+0.2 -0.5 |
+0.2 -0.5 |
+0.2 -0.5 |
||||
| 显气孔率%≤ | 22 | 24 | 26 | 24 | 26 | 24 | 26 | |
| 常温耐压强度MPa≥ | 30 | 25 | 20 | 20 | 15 | 20 | 15 | |
关键词:
黏土砖
获取报价